ASTM A681 | DIN | JIS | GB/T 1299 |
D2 / T30402 | 1.2436 | SKD11 | 4Cr5MoSiV |
C (%) | V(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Mo(%) | Cu(%) | Cr(%) | Ni(%) | Co, % |
1.45-1.60 | 0.50-1.10 | ≦0.60 | ≦0.60 | ≦0.030 | ≦0.020 | 11.00-13.00 | 0.70-1.20 | ≦0.25 | ≦0.25 | ≦0.25 | ≦1.00 |
Grade | Annealing delivery condition | Sample quenching hardness | ||
Hardness HBW | Quenching temperature | coolant | Rockwell hardness HRC | |
Cr12Mo1V1 | 255 max. | 820°C±15°C preheating, 1000°C(salt bath) ±6°C or 1010°C(furnace-controlling air) ±6°C heating, heat preservation 10-20min air cooling, 200°C ±6°C quenching,2 hour | 59 |
Katalor has overall quality assurance system, advanced producing and testing equipment to guarantee the products quality.
We offer various machining services such as cutting, CNC milling, grinding and heat treatment.
All mold steel products need to be tested before shipping.